GeneralDescription :
Al-Sr alloy is a kind of modifier used inAl-Si alloy casting for improving the mechanical properties (mainly impacttoughness) of Al-Si alloy.
In case of over-injected silicon material,it becomes very weak structured. Therefore the modifier can prevent thisproblem and even further, can help to achieve the uniformity and improvedstructure of the material.
Usages :
Aluminium Alloy A356.2 ingot,A319(AlSiCu3), A356(AlSi7Mg),
A413(AlSi12), A360(AlSi12Mg).
Vehicle Wheel.
Vehicle Engine Parts.
Advantages:
1) Higher returned rate.
2) Improving the efficiency for thefabrication.
3) Improving uniformity of the elements.
4) Reducing the porosity.
5) Improving efficiency of heat-treatment.
6) Improving surface treatment.
Instructions for use :
1. Preparethe required alloy composition. Follow the normal fluxing and cleaningprocedure as recommended.
2. Afterthe refining and separating operation, push the surface scum of liquid aluminumaside, according to the quantity to add the AlSr alloy at temperature between 720-740Deg C.
3. Afteradding AlSr alloy, aluminum alloy liquid has a tendency to absorb hydrogen, itis necessary to strengthen the degassing.
4. After AlSrmelting,that is, achieve the metamorphic effect, can be used to cast.
Specifications
Chemical Composition:
Products | Model | Compositions(Bal. Al) |
Al-Sr alloy modifier | AlSr5 | Sr4.0~6.0%,Si0.2%max,Fe0.3%max |
AlSr10 | Sr9.0~11%,Si0.2%max,Fe0.3%max | |
AlSr15 | Sr14~16%,Si0.2%max,Fe0.3%max | |
AlSr20 | Sr18~22%,Si0.2%max,Fe0.3%max |
Physical Specifications:
Cut rod:
Dia. =9.5~10.0mm, standard length500mm(100g), 1000mm(200g),1200mm(240g).
Dia. =20mm,AlSr15/AlSr20.
Waffle plate:
6-7kg/waffle ingot.
Packing:
1000kgs/pallet or wooden crate.
Storage:
Placed in ventilated and dry place,long-term preservation.